PE — Solid & Cellular Polyethylene Insulation and Jacketing
Low-permittivity thermoplastic polyolefin used as solid or cellular (foam) core dielectric for impedance-controlled data and fieldbus cables, and as carbon-black UV-resistant outdoor jacketing.
What is PE & Foam PE insulation?
Polyethylene (PE) is a non-polar, halogen-free polyolefin featuring remarkably low dielectric permittivity (~2.3 solid, ~1.4–1.6 when cellular/foamed) and minimal moisture absorption. Extruded as cellular (foam) PE around twisted-pair conductors, micro-cellular gas cells lower mutual capacitance and raise propagation velocity — making Foam PE the preferred dielectric for 120 Ω and 150 Ω industrial fieldbus, RS-485, CAN and high-speed differential data cables.
Compounded with finely dispersed carbon black as an outer sheath, medium- and high-density PE forms a tough, low-permeability barrier against solar UV radiation, standing water, soil chemistry and −40°C cold impact for outdoor solar telemetry, energy-storage yards and utility SCADA runs.
Across cable designs, density grade determines performance: low-density (LDPE) and cellular Foam PE maximise flexibility and signal velocity (~78%–82% velocity of propagation in foam twisted pairs), whereas medium- and high-density (MDPE/HDPE) carbon-black compounds (typically 2%–2.5% UV-stabilising carbon black) deliver tough, low-friction outdoor and direct-burial sheaths with minimal moisture ingress.
Two engineering limits define PE's application boundary: as a non-cross-linked thermoplastic, PE softens above ~105°C–130°C (capping continuous ratings around 70°C–80°C, above which cross-linked XLPE is required); and unmodified PE is combustible rather than flame-retardant, so outdoor PE-jacketed cables entering occupied buildings must transition to flame-retardant or LSZH indoor cabling within applicable NEC or EU CPR entry-distance limits.
Key Material Properties
| Property | Rating | Notes |
|---|---|---|
| Dielectric | εr ~2.3 (solid) · ~1.5 (foam) | Ultra-low mutual capacitance for serial data |
| Outdoor sheath | UV- & moisture-resistant (black PE) | Very low water-vapour permeability |
| Temperature | −40°C to +80°C typical | Halogen-free thermoplastic polyolefin |
| Typical uses | Fieldbus, RS-485, data pairs, outdoor jackets | Impedance-matched & weatherproof cables |
| Grades & Propagation | LDPE / Foam PE (cores) · Black MDPE/HDPE (sheaths) | 2%–2.5% carbon black for long-term UV stability |
| Fire & Thermal limits | Not inherently flame-retardant · ≤70°C–80°C cont. | Upgrade to XLPE for 90°C–150°C or LSZH indoors |
PE Insulated Products
- LI2YCY-TP — DIN VDE 0812 / DIN 47100 · PE · -40°C to +80°C · 250V
Applications & Standards Using This Material
Frequently Asked Questions
- Why do RS-485 and CAN fieldbus cables use Foam PE instead of PVC?
- Foaming polyethylene introduces microscopic gas cells that cut dielectric constant and mutual capacitance roughly in half compared with PVC, preventing signal edge rounding and reflections over long trunk lines.
- When is a black PE outer jacket preferred over PVC?
- Carbon-black UV-stabilised PE excels in permanent outdoor, rooftop, underground duct and damp utility environments where sunlight stability and moisture exclusion outweigh indoor flame-retardant PVC requirements.
- Can an outdoor black PE-jacketed cable be routed throughout an indoor commercial building?
- Generally no — standard black PE jacketing is formulated for UV and moisture exclusion rather than flame retardancy and does not meet indoor riser, plenum or EU CPR flame-propagation classes. Per NEC and European building codes, transition outdoor PE cables to flame-retardant or LSZH indoor cabling at the building entrance.
- When should engineers upgrade from thermoplastic PE to cross-linked XLPE?
- Upgrade to XLPE whenever conductor temperatures exceed 70°C–80°C (for 90°C–150°C continuous operation), whenever overload/short-circuit non-melting endurance is mandatory, or whenever environmental stress-crack resistance under hot mechanical load is required.