PTFE — Polytetrafluoroethylene Insulation
Premier high-temperature fluoropolymer rated to 200°C–260°C continuous — delivering near-universal chemical immunity and high dielectric strength in a thin, lightweight wall.
What is PTFE insulation?
Polytetrafluoroethylene (PTFE) is the benchmark high-performance fluoropolymer for extreme thermal and chemical environments. It combines a wide operating window (typically −65°C to +200°C with silver-plated copper, or +260°C with nickel-plated copper), virtual immunity to fuels, oils, acids and solvents, and outstanding dielectric stability in a slim, lightweight wall.
That performance profile makes PTFE a mainstay across aerospace airframe wires (such as AS 22759 and BS 3G 210), high-temperature hook-up wires (such as NEMA HP3 and UL AWM PTFE styles) and precision thermocouple cables. In weight-critical aircraft, instrumentation and hot-zone assemblies, thin-wall PTFE cuts harness mass while resisting soldering heat and aggressive fluids.
Engineers commonly start with PTFE when thermal, chemical and low-loss dielectric requirements rule out conventional thermoplastics and elastomers, then select the matching aerospace, NEMA or UL specification.
Key Material Properties
| Property | Rating | Notes |
|---|---|---|
| Max temperature | 200°C–260°C continuous | Plating dependent (−65°C low-temp class) |
| Type | Non-melt fluoropolymer | Thin, lightweight extruded or wrapped wall |
| Chemical resistance | Outstanding | Inert to fuels, oils, acids & solvents |
| Typical uses | Aerospace, military, NEMA HP, high-temp AWM | Weight- & heat-critical wiring |
PTFE Insulated Products
- UL 5256 — UL 758 AWM · PTFE / Glass serve · 250°C · 600V
- UL 5196 — UL 758 AWM · PTFE / Glass serve · 250°C · 600V
- UL 1213 — UL 758 AWM · PTFE · -60°C to +105°C
- UL 1199 — UL 758 AWM · PTFE · -60°C to +200°C · 600V
- UL 1180 — UL 758 AWM · PTFE · -60°C to +200°C · 300V
- SAE AS22759/12 — AS 22759 · PTFE · -55°C to +260°C · 600V
- SAE AS22759/11 — AS 22759 · PTFE · -55°C to +200°C · 600V
- SAE AS22759/10 — AS 22759 · PTFE · -55°C to +260°C · 1000V
- SAE AS22759/9 — AS 22759 · PTFE · -55°C to +200°C · 1000V
- NEMA HP 3 TYPE ET — NEMA HP3 · PTFE · -65°C to +200°C · 250V
- NEMA HP 3 TYPE EE — NEMA HP3 · PTFE · -65°C to +200°C · 1000V
- NEMA HP 3 TYPE E — NEMA HP3 · PTFE · -65°C to +200°C · 600V
- FLR5Y — ISO 19642-3 · PTFE · -40°C to +260°C · 25/60V
- BS 3G 210 TYPE C — BS 3G 210 · PTFE · -75°C to +190°C · 600V
- BS 3G 210 TYPE B — BS 3G 210 · PTFE · -75°C to +190°C · 300V
Applications & Standards Using This Material
Frequently Asked Questions
- Why is PTFE widely used for aerospace and high-temperature wire?
- PTFE combines a wide temperature envelope (up to 260°C), chemical and fuel inertness, soldering-heat resistance and high dielectric strength in a very thin, lightweight wall.
- What temperature can PTFE wire withstand continuously?
- Typically 200°C continuous with silver-plated copper conductors and up to 260°C continuous with nickel-plated copper, with low-temperature flexibility down to −65°C.
- How does PTFE compare to PVC?
- PTFE dramatically exceeds PVC in continuous temperature ceiling, chemical immunity and high-frequency dielectric performance, making it the choice for extreme environments where PVC degrades.
Engineering Guides
- High-Temperature Conductor Selection (150°C to 1000°C+): Tin, Silver, 2% Nickel, 27% Nickel-Coated & Pure Nickel — Why copper oxidizes and forms brittle intermetallics at elevated temperatures — and how to match ASTM B33, B298, B355 (Class 2 & 27), and B160 conductor metallurgies to operating temperature, DCR voltage drop, and permanent termination methods.
- Fluoropolymer vs. Silicone Insulation Guide: PTFE, FEP, PFA, ETFE, PVDF & SiR Tradeoffs — How to choose between extruded/wrapped PTFE, melt-processable FEP and PFA, mechanically tough ETFE and PVDF, and ultra-flexible Silicone Rubber across chemical immersion, bend radius, cut-through, max O.D., HV corona, and 2026 PFAS strategy.
- Why FEP & PTFE Insulated Cores Cannot Use Cross-Linked Jackets: E-Beam, Peroxide, Silane, and Silicone Compatibility Guide — Real failure-analysis photos and polymer-physics guide explaining why cross-linked PUR, rubber, and XLPE jackets cause brittle cracking and fracture in FEP/PTFE primary cores — plus safe hybrid alternatives.